Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Schüttdichte | 23.0 °C | 0.6 g/cm³ Show Material materials with Schüttdichte of 0.6 g/cm³ | ASTM D 1895 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 66 MPa Show Material materials with Biegefestigkeit of 66 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.63 GPa Show Material materials with Biegemodul of 3.63 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2 % Show Material materials with Dehnung of 2 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 2.99 GPa Show Material materials with Elastizitätsmodul of 2.99 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D256A |
Zugfestigkeit | 23.0 °C | 45 MPa Show Material materials with Zugfestigkeit of 45 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 7 g/10min Show Material materials with Schmelzmassenflussrate of 7 g/10min | ASTM D 1238 | 200°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Food Container |