Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Schüttdichte | 23.0 °C | 0.6 g/cm³ Show Material materials with Schüttdichte of 0.6 g/cm³ | ASTM D 1895 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 44 MPa Show Material materials with Biegefestigkeit of 44 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.65 GPa Show Material materials with Biegemodul of 2.65 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 50 % Show Material materials with Dehnung of 50 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 2.35 GPa Show Material materials with Elastizitätsmodul of 2.35 GPa | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 67 [-] Show Material materials with Hardness, Rockwell L of 67 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 110 J/m Show Material materials with Impact strength, Izod notched, ASTM of 110 J/m | ASTM D256A |
Zugfestigkeit | 23.0 °C | 29 MPa Show Material materials with Zugfestigkeit of 29 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 4 g/10min Show Material materials with Schmelzmassenflussrate of 4 g/10min | ASTM D 1238 | 230°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging |