Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.33 g/cm³ Show Material materials with Dichte of 1.33 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.14 % Show Material materials with Wasserabsorption of 0.14 % | ASTM D 570 | 24 Hours |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.6 % Show Material materials with Wasseraufnahme, Gleichgewicht of 0.6 % | ASTM D 570 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 68 MPa Show Material materials with Biegefestigkeit of 68 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.24 GPa Show Material materials with Biegemodul of 2.24 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 120 % Show Material materials with Dehnung of 120 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 68 MPa Show Material materials with Flexural yield strength of 68 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Material materials with Hardness, Rockwell R of 115 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | -40.0 °C | 170 J/m Show Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 |
-30.0 °C | 192 J/m Show Material materials with Impact strength, Izod notched, ASTM of 192 J/m | ASTM D 256 | |
23.0 °C | 640 J/m Show Material materials with Impact strength, Izod notched, ASTM of 640 J/m | ASTM D 256 | |
Streckgrenze | 23.0 °C | 41 MPa Show Material materials with Streckgrenze of 41 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 41 MPa Show Material materials with Zugfestigkeit of 41 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 121 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.28E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.28E-5 1/K | ASTM E 831 | 60°C to 138°C | ||
Relative temperature index, electrical | 105 °C Show Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating | 2.2mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 5.7 [-] Show Material materials with Dielektrizitätskonstante of 5.7 [-] | ASTM D 150 | at 1 MHz |
Durchschlagfestigkeit | 23.0 °C | 12 kV/mm Show Material materials with Durchschlagfestigkeit of 12 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Material materials with Kriechstromfestigkeit of 3 V | UL 746A |
Verlustfaktor | 23.0 °C | 0.03 [-] Show Material materials with Verlustfaktor of 0.03 [-] | ASTM D 150 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 1 - 1.4 % Show Material materials with Schrumpfung of 1 - 1.4 % | SABIC method | 2.3-4.6 mm |
Schrumpfung, diagonal | 23.0 °C | 1.2 - 1.6 % Show Material materials with Schrumpfung, diagonal of 1.2 - 1.6 % | SABIC method | 2.3-4.6 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Heavy Vehicles,Medical Device,Personal Computing,Surgical Devices,Wireless Communications | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 50-75°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |