Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.53 g/cm³ Show Material materials with Dichte of 1.53 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.06 % Show Material materials with Wasserabsorption of 0.06 % | ASTM D 570 | 24 Hours |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 190 MPa Show Material materials with Biegefestigkeit of 190 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 7.58 GPa Show Material materials with Biegemodul of 7.58 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 3 % Show Material materials with Dehnung of 3 % | ASTM D 638 | Type I, 5 mm/min |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 801 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 801 J/m | ASTM D 4812 |
Zugfestigkeit | 23.0 °C | 119 MPa Show Material materials with Zugfestigkeit of 119 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 207 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 207 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.52E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.52E-5 1/K | ASTM E 831 | 60°C to 138°C | ||
Relative temperature index, electrical | 140 °C Show Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 140 °C Show Material materials with Relative temperature index, mechanical impact of 140 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating | 0.83mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 3.7 [-] Show Material materials with Dielektrizitätskonstante of 3.7 [-] | ASTM D 150 | at 1 MHz |
Durchschlagfestigkeit | 23.0 °C | 24 kV/mm Show Material materials with Durchschlagfestigkeit of 24 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Kriechstromfestigkeit | 23.0 °C | 0 V Show Material materials with Kriechstromfestigkeit of 0 V | UL 746A |
Verlustfaktor | 23.0 °C | 0.02 [-] Show Material materials with Verlustfaktor of 0.02 [-] | ASTM D 150 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 - 0.8 % Show Material materials with Schrumpfung of 0.5 - 0.8 % | SABIC method | 3.2-4.6 mm |
Schrumpfung, diagonal | 23.0 °C | 0.6 - 0.9 % Show Material materials with Schrumpfung, diagonal of 0.6 - 0.9 % | SABIC method | 3.2-4.6 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Auto Aftermarket,Circuit Protection,Data Management,Data Transfer,Defense Vehicles,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exercise Equipment,Fixture Bath/Shower,Forward Lighting,Heavy Vehicles,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Meter Water,Modular Panel,Monitoring and Imaging,Non-LED Lighting,Oil/Gas,Personal Care,Personal Computing,Photovoltaic Components,Plumbing,Power Manangement,Pump,Recreational Vehicle,Refrigerator,Security/Detection,Semiconductor,Small Appliance,Storage/Table,Surgical Devices,Swimming Pool/Spa,Vacuum Cleaner,Water Treatment/Filtration,Weaving Machine,Wireless Communications,Wiring Devices | |
Fillers | 30% Glass Fiber | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |