Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Material materials with Dichte of 1.19 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.07 % Show Material materials with Wasserabsorption of 0.07 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.3 GPa Show Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 102 % Show Material materials with Dehnung of 102 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.25 GPa Show Material materials with Elastizitätsmodul of 2.25 GPa | ASTM D 638 | 50 mm/min |
Elongation at yield | 23.0 °C | 5.7 % Show Material materials with Elongation at yield of 5.7 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 92 MPa Show Material materials with Flexural yield strength of 92 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 230 J/m Show Material materials with Impact strength, Izod notched, ASTM of 230 J/m | ASTM D 256 |
23.0 °C | 740 J/m Show Material materials with Impact strength, Izod notched, ASTM of 740 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | -30.0 °C | 2000 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 2000 J/m | ASTM D 4812 |
23.0 °C | 2150 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 2150 J/m | ASTM D 4812 | |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 16 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | ISO 179/1eA |
23.0 °C | 50 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 50 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30.0 °C | 134 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 134 kJ/m² | ISO 179/1eU |
23.0 °C | 135 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 135 kJ/m² | ISO 179/1eU | |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 21 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 21 kJ/m² | ISO 180/1A |
23.0 °C | 58 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 58 kJ/m² | ISO 180/1A | |
Schlagzähigkeit, Izod ungekerbt | -30.0 °C | 183 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 183 kJ/m² | ISO 180/1U |
23.0 °C | 184 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 184 kJ/m² | ISO 180/1U | |
Streckgrenze | 23.0 °C | 56 MPa Show Material materials with Streckgrenze of 56 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 51 MPa Show Material materials with Zugfestigkeit of 51 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 118 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 118 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.9E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Vicat-Erweichungstemperatur | 136 °C Show Material materials with Vicat-Erweichungstemperatur of 136 °C | ASTM D 1525 | Rate B/50 | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.1E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Compliant, 94-5VB Rating | 2mm | UL 94 by SABIC-IP |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.8 [-] Show Material materials with Dielektrizitätskonstante of 2.8 [-] | SABIC method | at 10 GHz |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Material materials with Kriechstromfestigkeit of 3 V | UL 746A |
Verlustfaktor | 23.0 °C | 5.2E-3 [-] Show Material materials with Verlustfaktor of 5.2E-3 [-] | SABIC method | at 10 GHz |
Volume resistivity | 23.0 °C | 1.00E+16 - 1.00E+17 Ω·cm Show Material materials with Volume resistivity of 1.00E+16 - 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 30 g/10min Show Material materials with Schmelzmassenflussrate of 30 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Schmelzvolumenflussrate | 29 cm³/10min Show Material materials with Schmelzvolumenflussrate of 29 cm³/10min | ISO 1133 | 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.6 - 0.8 % Show Material materials with Schrumpfung of 0.6 - 0.8 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.6 - 0.8 % Show Material materials with Schrumpfung, diagonal of 0.6 - 0.8 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine,Audio,Circuit Protection,Data Transfer,Displays,Enclosure/Housing/Cover,Enclosures,EV Infrastructure,LED Lighting,Non-LED Lighting,Personal Computing,Power Manangement,Wireless Communications | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 270-295°C, Nozzle Temperature: 265-290°C, Front - Zone 3 Temperature: 270-295°C, Middle - Zone 2 Temperature: 260-280°C, Rear - Zone 1 Temperature: 250-270°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |