Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 0.902 g/cm³ Show Material materials with Dichte of 0.902 g/cm³ | ASTM D1505 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.08232 GPa Show Material materials with Biegemodul of 0.08232 GPa | ASTM D790 |
Dehnung | 800.0 % Show Material materials with Dehnung of 800.0 % | ASTM D638 |
Zugfestigkeit | 24.5 MPa Show Material materials with Zugfestigkeit of 24.5 MPa | ASTM D638 |
Thermisch
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 4.0 % Show Material materials with Opazität of 4.0 % | ASTM D1003 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Mooney-Viskosität | 20.0 MU Show Material materials with Mooney-Viskosität of 20.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | General purpose film,Lamination film |