Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 0.902 g/cm³ Show Material materials with Dichte of 0.902 g/cm³ | ASTM D1505 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.0744799999999999 GPa Show Material materials with Biegemodul of 0.0744799999999999 GPa | ASTM D790 |
Dehnung | 850.0 % Show Material materials with Dehnung of 850.0 % | ASTM D638 |
Zugfestigkeit | 19.6 MPa Show Material materials with Zugfestigkeit of 19.6 MPa | ASTM D638 |
Thermisch
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 0.5 % Show Material materials with Opazität of 0.5 % | ASTM D1003 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Mooney-Viskosität | 10.0 MU Show Material materials with Mooney-Viskosität of 10.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Stretch film,General purpose film,Lamination film |