Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 1.2 [-] Show Material materials with Coefficient of friction of 1.2 [-] | ASTM D1894 | |
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 13 % Show Material materials with Opazität of 13 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE. |