Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
SABIC® LLDPE 118P
SABIC® LLDPE 118P is a butene linear low density polyethylene resin typically used for food applications. It contains an antioxidant inspired by nature offering advantages versus conventional stabilizers: - Produced with no phosphorus or sulphur based additives - Improved processing stability at a much reduced concentration - No Specific Migration Limit (SML free) Films produced from this resin typically have good puncture resistance, high tensile strength, good hot tack properties and low gel levels. Typical applications for SABIC® LLDPE 118P are (frozen) food bags and lamination films. Film properties. Film of 50 μm and BUR=2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationAllgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 1.2 [-] Show Material materials with Coefficient of friction of 1.2 [-] | ASTM D1894 | |
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 13 % Show Material materials with Opazität of 13 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | It is used in food applications (frozen food bags and lamination films). |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.