Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.93 g/cm³ Show Material materials with Dichte of 0.93 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 850 % Show Material materials with Dehnung of 850 % | ASTM D638 |
Elongation at yield | 23.0 °C | 12 % Show Material materials with Elongation at yield of 12 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 48 [-] Show Material materials with Härte, Shore D of 48 [-] | ASTM D2240 |
Streckgrenze | 23.0 °C | 14 MPa Show Material materials with Streckgrenze of 14 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 25 MPa Show Material materials with Zugfestigkeit of 25 MPa | ASTM D638 |
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | Electrical,Wire & cable |