Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.17 [-] Show Material materials with Dielektrizitätskonstante of 2.17 [-] | ASTM D150 | at 60 Hz |
Durchschlagfestigkeit | 23.0 °C | 55 kV/mm Show Material materials with Durchschlagfestigkeit of 55 kV/mm | ASTM D149 | at 500 V/sec |
Verlustfaktor | 23.0 °C | 1000 [-] Show Material materials with Verlustfaktor of 1000 [-] | ASTM D150 | at 60 Hz |
spezifischer Widerstand | 23.0 °C | 5.00E+13 Ω·m Show Material materials with spezifischer Widerstand of 5.00E+13 Ω·m | ASTM D257 |
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 1.2 % Show Material materials with Opazität of 1.2 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Stretch film,Masterbatch,Wire & cable,General purpose film,Cast film |