Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Material materials with Dichte of 1.19 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.3 % Show Material materials with Wasserabsorption of 0.3 % | ISO 62 | 24 Hours |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 135 MPa Show Material materials with Biegefestigkeit of 135 MPa | ISO 178 |
Biegemodul | 23.0 °C | 3.3 GPa Show Material materials with Biegemodul of 3.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 7 % Show Material materials with Dehnung of 7 % | ISO 527 |
Elastizitätsmodul | 23.0 °C | 3.3 GPa Show Material materials with Elastizitätsmodul of 3.3 GPa | ISO 527 |
Härte, Rockwell M | 23.0 °C | 95 [-] Show Material materials with Härte, Rockwell M of 95 [-] | ISO 2039 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 1.4 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 1.4 kJ/m² | ISO 179 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 20 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 20 kJ/m² | ISO 179/1eU |
Zugfestigkeit | 23.0 °C | 75 MPa Show Material materials with Zugfestigkeit of 75 MPa | ISO 527 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 93 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 93 °C | ISO 75-1&2 | 1.8 MPa | |
Vicat-Erweichungstemperatur | 100 °C Show Material materials with Vicat-Erweichungstemperatur of 100 °C | ISO 306 | B50 | |
Wärmeleitfähigkeit | 23.0 °C | 0.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.2 W/(m·K) | ASTM C177 |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Optisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 2.3 g/10min Show Material materials with Schmelzmassenflussrate of 2.3 g/10min | ISO 1133 | 230°C/3.8 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Lighting |