Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
SABIC® LDPE 2501N0W is a grade without additives with a low gel level, which combines good draw down ability with fair optical properties and stiffness. Application SABIC® LDPE 2501N0W is typically used in diaper film, surface protection film, lamination film and in applications where low blocking behavior is required and the presence of slip and anti block is unwanted. SABIC® LDPE 2501N0W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 50 μm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationAllgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.9 [-] Show Material materials with Coefficient of friction of 0.9 [-] | ASTM D1894 | |
Dichte | 23.0 °C | 0.93 g/cm³ Show Material materials with Dichte of 0.93 g/cm³ | ASTM D1505 |
Mechanisch
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 10 % Show Material materials with Opazität of 10 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for film and lamination applications |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.