Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.65 % Show Material materials with Wasserabsorption of 0.65 % | ISO 62 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.8 GPa Show Material materials with Biegemodul of 2.8 GPa | ISO 178 |
Elastizitätsmodul | 23.0 °C | 2.9 GPa Show Material materials with Elastizitätsmodul of 2.9 GPa | ISO 527-2 1A | 1mm/min |
Elongation at yield | 23.0 °C | 7.5 % Show Material materials with Elongation at yield of 7.5 % | ISO 527-2 1A | 50mm/min |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 120 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 120 kJ/m² | ISO 179/1eU |
23.0 °C | 120 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 120 kJ/m² | ISO 179/1eU | |
Streckgrenze | 23.0 °C | 65 MPa Show Material materials with Streckgrenze of 65 MPa | ISO 527-2 1A | 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 106 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 106 °C | ISO 75-1&2 | 1.8 MPa | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-4 1/K | ISO 11359-2 |
Schmelzpunkt | 166 °C Show Material materials with Schmelzpunkt of 166 °C | ISO 11357-1/-3 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 24 cm³/10min Show Material materials with Schmelzvolumenflussrate of 24 cm³/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 1.9 % Show Material materials with Schrumpfung of 1.9 % | ISO 294-4 |
Schrumpfung, diagonal | 23.0 °C | 1.8 % Show Material materials with Schrumpfung, diagonal of 1.8 % | ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive |