Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.5 GPa Show Material materials with Biegemodul of 2.5 GPa | ISO 178 |
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527-2 1A | 1mm/min |
Elongation at yield | 23.0 °C | 11 % Show Material materials with Elongation at yield of 11 % | ISO 527-2 1A | 50mm/min |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8.5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8.5 kJ/m² | ISO 179/1eA |
Streckgrenze | 23.0 °C | 61 MPa Show Material materials with Streckgrenze of 61 MPa | ISO 527-2 1A | 50 mm/min |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 2.5 cm³/10min Show Material materials with Schmelzvolumenflussrate of 2.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive |