Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.2 [-] Show Material materials with Dielektrizitätskonstante of 2.2 [-] | ASTM D150 | at 60 Hz |
Verlustfaktor | 23.0 °C | 5E-4 [-] Show Material materials with Verlustfaktor of 5E-4 [-] | ASTM D150 | at 60 Hz |
spezifischer Widerstand | 23.0 °C | 8.50E+13 Ω·m Show Material materials with spezifischer Widerstand of 8.50E+13 Ω·m | ASTM D257 |
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 2.1 % Show Material materials with Opazität of 2.1 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Typically used for low filled or additive masterbatches in film and blow moulding applications(e.g. slip agents, anti fog agents, anti static agents, thermal stabilizers). |