Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Härte, Shore D | 23.0 °C | 53 [-] Show Material materials with Härte, Shore D of 53 [-] | ISO 868 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.2 [-] Show Material materials with Dielektrizitätskonstante of 2.2 [-] | ASTM D150 | at 60 Hz |
Verlustfaktor | 23.0 °C | 5E-4 [-] Show Material materials with Verlustfaktor of 5E-4 [-] | ASTM D150 | at 60 Hz |
spezifischer Widerstand | 23.0 °C | 8.50E+13 Ω·m Show Material materials with spezifischer Widerstand of 8.50E+13 Ω·m | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for wire and cable applications (telecommunication and power cable (LV, MV, HV) jacketing, halogen-free flame retardant (HFFR) compounds, one-step or two-steps silane crosslinkable for cable insulation). |