Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Härte, Shore D | 23.0 °C | 53 [-] Show Material materials with Härte, Shore D of 53 [-] | ISO 868 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 121 °C Show Material materials with Schmelzpunkt of 121 °C | SABIC method |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.2 [-] Show Material materials with Dielektrizitätskonstante of 2.2 [-] | ASTM D150 | at 60 Hz |
Durchschlagfestigkeit | 23.0 °C | 55 kV/mm Show Material materials with Durchschlagfestigkeit of 55 kV/mm | ASTM D149 | at 500 V/sec |
Verlustfaktor | 23.0 °C | 5E-4 [-] Show Material materials with Verlustfaktor of 5E-4 [-] | ASTM D150 | at 60 Hz |
spezifischer Widerstand | 23.0 °C | 8.50E+13 Ω·m Show Material materials with spezifischer Widerstand of 8.50E+13 Ω·m | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable |