Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.63 g/cm³ Show Material materials with Dichte of 1.63 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.07 % Show Material materials with Wasserabsorption of 0.07 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 180 MPa Show Material materials with Biegefestigkeit of 180 MPa | ISO 178 |
Biegemodul | 23.0 °C | 9.5 GPa Show Material materials with Biegemodul of 9.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Material materials with Dehnung of 2 % | ASTM D 638 | Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12 GPa Show Material materials with Elastizitätsmodul of 12 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ASTM D 638 | Type I, 5 mm/min |
Hardness, Ball Indentation | 23.0 °C | 118 MPa Show Material materials with Hardness, Ball Indentation of 118 MPa | ISO 2039-1 |
Hardness, Rockwell R | 23.0 °C | 119 [-] Show Material materials with Hardness, Rockwell R of 119 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | -30.0 °C | 57 J/m Show Material materials with Impact strength, Izod notched, ASTM of 57 J/m | ASTM D 256 |
23.0 °C | 60 J/m Show Material materials with Impact strength, Izod notched, ASTM of 60 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 620 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 620 J/m | ASTM D 4812 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA |
23.0 °C | 7 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30.0 °C | 50 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | ISO 179/1eU |
23.0 °C | 50 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | ISO 179/1eU | |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 6 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1A |
23.0 °C | 7 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180/1A | |
Schlagzähigkeit, Izod ungekerbt | -30.0 °C | 45 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 45 kJ/m² | ISO 180/1U |
23.0 °C | 45 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 45 kJ/m² | ISO 180/1U | |
Streckgrenze | 23.0 °C | 120 MPa Show Material materials with Streckgrenze of 120 MPa | ASTM D 638 | Type I, 5 mm/min |
Zugfestigkeit | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit of 120 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 200 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 200 °C Show Material materials with Vicat-Erweichungstemperatur of 200 °C | ASTM D 1525 | Rate B/50 | |||
Wärmeleitfähigkeit | 23.0 °C | 0.25 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.25 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.9E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.9E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating | 2mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 3.7 [-] Show Material materials with Dielektrizitätskonstante of 3.7 [-] | ASTM D 150 | at 1 MHz |
Durchschlagfestigkeit | 23.0 °C | 24 kV/mm Show Material materials with Durchschlagfestigkeit of 24 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Kriechstromfestigkeit | 23.0 °C | 175 V Show Material materials with Kriechstromfestigkeit of 175 V | IEC 60112 |
Verlustfaktor | 23.0 °C | 0.02 [-] Show Material materials with Verlustfaktor of 0.02 [-] | ASTM D 150 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 42 g/10min Show Material materials with Schmelzmassenflussrate of 42 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Schmelzvolumenflussrate | 29 cm³/10min Show Material materials with Schmelzvolumenflussrate of 29 cm³/10min | ISO 1133 | 250°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 - 0.7 % Show Material materials with Schrumpfung of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.5 - 1 % Show Material materials with Schrumpfung, diagonal of 0.5 - 1 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Air Conditioning,ATM/Ticket Machine,Audio,Auto Aftermarket,Building Accessory,Circuit Protection,Cladding,Cladding/Roof,Coffee Maker/Espresso Machine,Commercial Storage/Cookware,Cooking Range,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exterior Mirror,Food Processor,Forward Lighting,Gas/Electric Oven,Heavy Vehicles,HVAC Underhood,Industrial Material Handling,Lab Ware and Clinical Diagnostics,Laundry Dryer,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Meter Water,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Personal Care,Personal Computing,Photovoltaic Components,Pipe/Fitting,Plumbing,Power Boat,Power Manangement,Pump,Recreational Vehicle,Refrigerator,Security/Detection,Small Appliance,Toy,Vacuum Cleaner,Water Treatment/Filtration,Wearables,Wireless Communications,Wiring Devices,Wire & cable | |
Fillers | 30% Glass Fiber | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 255-275°C, Nozzle Temperature: 250-270°C, Front - Zone 3 Temperature: 255-275°C, Middle - Zone 2 Temperature: 250-270°C, Rear - Zone 1 Temperature: 245-265°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |