Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.91 g/cm³ Show Material materials with Dichte of 0.91 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.4 GPa Show Material materials with Biegemodul of 1.4 GPa | ASTM D790 A |
Hardness, Rockwell L | 23.0 °C | 95 [-] Show Material materials with Hardness, Rockwell L of 95 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | -20.0 °C | 35 J/m Show Material materials with Impact strength, Izod notched, ASTM of 35 J/m | ASTM D256 |
23.0 °C | 65 J/m Show Material materials with Impact strength, Izod notched, ASTM of 65 J/m | ASTM D256 | |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Houseware & appliances,Furniture |