Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.15 GPa Show Material materials with Biegemodul of 1.15 GPa | ASTM D790 A |
Hardness, Rockwell L | 23.0 °C | 80 [-] Show Material materials with Hardness, Rockwell L of 80 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | -20.0 °C | 63 J/m Show Material materials with Impact strength, Izod notched, ASTM of 63 J/m | ASTM D256 |
23.0 °C | 115 J/m Show Material materials with Impact strength, Izod notched, ASTM of 115 J/m | ASTM D256 | |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Houseware & appliances |