Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.91 g/cm³ Show Material materials with Dichte of 0.91 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.8 GPa Show Material materials with Biegemodul of 1.8 GPa | ASTM D790 A |
Elongation at yield | 23.0 °C | 11 % Show Material materials with Elongation at yield of 11 % | ISO 527-1/-2 |
Hardness, Rockwell L | 23.0 °C | 104 [-] Show Material materials with Hardness, Rockwell L of 104 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 20 J/m Show Material materials with Impact strength, Izod notched, ASTM of 20 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 35 MPa Show Material materials with Streckgrenze of 35 MPa | ASTM D638 |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Thin wall packaging |