Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
SABIC® SUPEER™ 7318BE
SABIC® SUPEER™ 7318BE is a metallocene ethylene-hexene copolymer. It has a good processability and performs well in a wide range of general purpose and high performance cast film applications. Films produced with this grade offer good impact strength, puncture resistance, sealing and optical properties. SABIC® SUPEER™ 7318BE is typically used for stretch and lamination films. Processing temperatures 210- 260 °C. Properties have been measured on cast film of 25 µm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationMechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Reißfestigkeit | 23.0 °C | 137.2 kN/m Show Material materials with Reißfestigkeit of 137.2 kN/m | ASTM D1922 |
Reißfestigkeit, transversal | 23.0 °C | 166.6 kN/m Show Material materials with Reißfestigkeit, transversal of 166.6 kN/m | ASTM D1922 |
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 4 % Show Material materials with Opazität of 4 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Stretch and lamination films. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.