Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.48 g/cm³ Show Material materials with Dichte of 1.48 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 4 GPa Show Material materials with Biegemodul of 4 GPa | ISO 178 |
Dehnung | 23.0 °C | 3.5 % Show Material materials with Dehnung of 3.5 % | ISO 527-2 1A | 5mm/min |
Elastizitätsmodul | 23.0 °C | 4 GPa Show Material materials with Elastizitätsmodul of 4 GPa | ISO 527-2 1A | 1mm/min |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 35 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | ISO 179/1eU |
Zugfestigkeit | 23.0 °C | 90 MPa Show Material materials with Zugfestigkeit of 90 MPa | ISO 527-2 1A | 5mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ISO 75-1&2 | 1.8 MPa | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6E-5 1/K | ISO 11359-2 |
Schmelzpunkt | 166 °C Show Material materials with Schmelzpunkt of 166 °C | ISO 11357-1/-3 | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.2E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.2E-4 1/K | ISO 11359-2 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 4.5 cm³/10min Show Material materials with Schmelzvolumenflussrate of 4.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive | |
Fillers | 10% Glass Fiber |