Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 95 MPa Show Material materials with Biegefestigkeit of 95 MPa | ISO 178 | 12.5 mm/min |
Biegemodul | 23.0 °C | 2.25 GPa Show Material materials with Biegemodul of 2.25 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 110 % Show Material materials with Dehnung of 110 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.3 GPa Show Material materials with Elastizitätsmodul of 2.3 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 6 % Show Material materials with Elongation at yield of 6 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 101 MPa Show Material materials with Flexural yield strength of 101 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 796 J/m Show Material materials with Impact strength, Izod notched, ASTM of 796 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 18 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 18 kJ/m² | ISO 180/1A |
23.0 °C | 70 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 70 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 64 MPa Show Material materials with Streckgrenze of 64 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 62 MPa Show Material materials with Zugfestigkeit of 62 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 125 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 125 °C Show Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 115 °C Show Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 142 °C Show Material materials with Vicat-Erweichungstemperatur of 142 °C | ASTM D 1525 | Rate B/50 | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.7E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating | 1.5mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 3 V Show Material materials with Kriechstromfestigkeit of 3 V | UL 746A |
Optisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 6.3 g/10min Show Material materials with Schmelzmassenflussrate of 6.3 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Schmelzvolumenflussrate | 7 cm³/10min Show Material materials with Schmelzvolumenflussrate of 7 cm³/10min | ISO 1133 | 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.6 - 0.8 % Show Material materials with Schrumpfung of 0.6 - 0.8 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management,Document Handling,Enclosures,Energy Management,Industrial Material Handling,LED Lighting,Meter Gas,Non-LED Lighting,Security/Detection | |
Processing methods | Drying Temperature: 120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 280-310°C, Nozzle Temperature: 270-290°C, Front - Zone 3 Temperature: 280-310°C, Middle - Zone 2 Temperature: 270-290°C, Rear - Zone 1 Temperature: 260-280°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-110°C |