Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.95 g/cm³ Show Material materials with Dichte of 0.95 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 1.25 GPa Show Material materials with Elastizitätsmodul of 1.25 GPa | ASTM D638 |
Elongation at yield | 23.0 °C | 10 % Show Material materials with Elongation at yield of 10 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 62 [-] Show Material materials with Härte, Shore D of 62 [-] | ASTM D2240 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 90 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 90 kJ/m² | ISO 8256 |
Streckgrenze | 23.0 °C | 27 MPa Show Material materials with Streckgrenze of 27 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Application areas | Jerry cans |