Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.95 g/cm³ Show Material materials with Dichte of 0.95 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 1.05 GPa Show Material materials with Elastizitätsmodul of 1.05 GPa | ASTM D638 |
Elongation at yield | 23.0 °C | 10 % Show Material materials with Elongation at yield of 10 % | ISO 527-1/-2 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 36 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 36 kJ/m² | ISO 179 |
Streckgrenze | 23.0 °C | 26 MPa Show Material materials with Streckgrenze of 26 MPa | ASTM D638 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 6.5 g/10min Show Material materials with Schmelzmassenflussrate of 6.5 g/10min | ISO 1133 | 190°C/21.6 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Jerry cans |