Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.95 g/cm³ Show Material materials with Dichte of 0.95 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 1.05 GPa Show Material materials with Elastizitätsmodul of 1.05 GPa | ISO 527 |
Härte, Shore D | 23.0 °C | 60 [-] Show Material materials with Härte, Shore D of 60 [-] | ISO 868 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 10 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180 |
23.0 °C | 22 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 22 kJ/m² | ISO 180 | |
Streckgrenze | 23.0 °C | 25 MPa Show Material materials with Streckgrenze of 25 MPa | ISO 527 |
Zugfestigkeit | 23.0 °C | 35 MPa Show Material materials with Zugfestigkeit of 35 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 73 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 73 °C | ISO 75 |
Schmelzpunkt | 132 °C Show Material materials with Schmelzpunkt of 132 °C | ISO 11357-1/-3 |
Vicat-Erweichungstemperatur | 126 °C Show Material materials with Vicat-Erweichungstemperatur of 126 °C | ISO 306 | 10N (VST/A) |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.32 g/10min Show Material materials with Schmelzmassenflussrate of 0.32 g/10min | ISO 1133 | 190°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for blow molding floaters for floating photovoltaic (PV) panel systems. Also used for large size containers (water tanks, transportation containers). |