Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.96 g/cm³ Show Material materials with Dichte of 0.96 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 1.35 GPa Show Material materials with Elastizitätsmodul of 1.35 GPa | ASTM D638 |
Elongation at yield | 23.0 °C | 7.5 % Show Material materials with Elongation at yield of 7.5 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 64 [-] Show Material materials with Härte, Shore D of 64 [-] | ASTM D2240 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 6.5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6.5 kJ/m² | ISO 179 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 75 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 75 kJ/m² | ISO 8256 |
Streckgrenze | 23.0 °C | 28 MPa Show Material materials with Streckgrenze of 28 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Application areas | Bottles |