Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 28 MPa Show Material materials with Biegefestigkeit of 28 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.1 GPa Show Material materials with Biegemodul of 1.1 GPa | ISO 178/1A |
Dehnung | 23.0 °C | 500 % Show Material materials with Dehnung of 500 % | ASTM D638 |
Härte, Shore D | 23.0 °C | 66 [-] Show Material materials with Härte, Shore D of 66 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 30 MPa Show Material materials with Streckgrenze of 30 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 18 MPa Show Material materials with Zugfestigkeit of 18 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 127 °C Show Material materials with Vicat-Erweichungstemperatur of 127 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Bottles |