Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 0.857 g/cm³ Show Material materials with Dichte of 0.857 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.0044 GPa Show Material materials with Biegemodul of 0.0044 GPa | ASTM D790 A | (1% Secant) |
Reißfestigkeit | 27.5 kN/m Show Material materials with Reißfestigkeit of 27.5 kN/m | ASTM D624 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Mooney-Viskosität | 24.0 MU Show Material materials with Mooney-Viskosität of 24.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable,Impact modification |