Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 0.868 g/cm³ Show Material materials with Dichte of 0.868 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.0132 GPa Show Material materials with Biegemodul of 0.0132 GPa | ASTM D790 A | (1% Secant) |
Reißfestigkeit | 39.2 kN/m Show Material materials with Reißfestigkeit of 39.2 kN/m | ASTM D624 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Mooney-Viskosität | 22.0 MU Show Material materials with Mooney-Viskosität of 22.0 MU | ASTM D1646 | ML 1+4, 121 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable,Impact modification |