Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.15 g/cm³ Show Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.2 % Show Material materials with Wasserabsorption of 0.2 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 2.3 GPa Show Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 100 % Show Material materials with Dehnung of 100 % | ISO 527 | 5 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527 | 1 mm/min | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527 | 50 mm/min | ||
Flexural yield strength | 23.0 °C | 80 MPa Show Material materials with Flexural yield strength of 80 MPa | ISO 178 | 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 96 MPa Show Material materials with Hardness, Ball Indentation of 96 MPa | ISO 2039-1 | ||
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Material materials with Hardness, Rockwell R of 115 [-] | ISO 2039-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 18 - 30 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 18 - 30 kJ/m² | ISO 179/1eA | ||
23.0 °C | 45 - 50 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 45 - 50 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 20 - 30 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 20 - 30 kJ/m² | ISO 180/1A | ||
23.0 °C | 40 - 50 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 40 - 50 kJ/m² | ISO 180/1A | |||
Streckgrenze | 23.0 °C | 55 MPa Show Material materials with Streckgrenze of 55 MPa | ISO 527 | 50 mm/min | ||
Zugfestigkeit | 23.0 °C | 45 MPa Show Material materials with Zugfestigkeit of 45 MPa | ISO 527 | 50 mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-30°C | ISO 179/1eU | ||||
Schlagzähigkeit, Izod ungekerbt | No Break @ 23,-30°C| ISO 180/1U |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 108 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 108 °C | ISO 75/Ae | 1.8 MPa | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 105 °C Show Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 134 °C Show Material materials with Vicat-Erweichungstemperatur of 134 °C | ISO 306 | Rate B/120 | |||
Wärmeleitfähigkeit | 23.0 °C | 0.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.2 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating 2nd value | 3mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.8 [-] Show Material materials with Dielektrizitätskonstante of 2.8 [-] | IEC 60250 | at 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 17 kV/mm Show Material materials with Durchschlagfestigkeit of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Kriechstromfestigkeit | 23.0 °C | 250 V Show Material materials with Kriechstromfestigkeit of 250 V | IEC 60112 |
Verlustfaktor | 23.0 °C | 7E-3 [-] Show Material materials with Verlustfaktor of 7E-3 [-] | IEC 60250 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 22 cm³/10min Show Material materials with Schmelzvolumenflussrate of 22 cm³/10min | ISO 1133 | 260°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 - 0.7 % Show Material materials with Schrumpfung of 0.5 - 0.7 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Amusement Machine,Applique,ATM/Ticket Machine,Audio,Auto Aftermarket,Body Protection,Building Accessory,Building Element,Circuit Protection,Cluster,Coffee Maker/Espresso Machine,Console,Cooking Range,Data Management,Data Transfer,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exterior Mirror,Exterior Trim,Exterior,Fluid Delivery,Food Processor,Food Transportation,Forward Lighting,Freezer,Front Grille,Fused Deposition Modeling (FDM),Gas/Electric Oven,Glove Box,Head Protection,Heavy Vehicles,HVAC Underhood,Industrial Material Handling,Infotainment/Telematic,Interior,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,LED Lighting,Long Distance Coach,Medical Device,Meter Gas,Meter Water,Modular Panel,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Overhead,Personal Care,Personal Computing,Personal Water Craft,Pharmaceutical Manufacturing,Pharmaceutical Packaging & Drug Delivery,Photo/Video Camera,Photovoltaic Components,Plumbing,Power Boat,Power Manangement,Rail Cabin Interiors,Rear/Signal Lighting,Recreational Vehicle,Refrigerator,Renal and Blood Handling,Respiratory,Safety Glasses,Seat,Security/Detection,Semiconductor,Small Appliance,Spoiler,Structure,Surgical Devices,Toy,Trim,Vacuum Cleaner,Vending Machine,Washing Machine,Watch/Jewelry,Wearables,Window,Wireless Communications,Wiring Devices,Wire & cable | |
Processing methods | Drying Temperature: 100-110°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 275-300°C, Nozzle Temperature: 275-300°C, Front - Zone 3 Temperature: 260-300°C, Middle - Zone 2 Temperature: 255-295°C, Rear - Zone 1 Temperature: 250-290°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 30-80%, Vent Depth: 0.038-0.076mm |