Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.18 g/cm³ Show Material materials with Dichte of 1.18 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.1 % Show Material materials with Wasserabsorption of 0.1 % | ASTM D 570 | 24 Hours |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 90 MPa Show Material materials with Biegefestigkeit of 90 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 2.35 GPa Show Material materials with Biegemodul of 2.35 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 157 % Show Material materials with Dehnung of 157 % | SABIC - Japan Method |
Impact strength, Izod notched, ASTM | 23.0 °C | 580 J/m Show Material materials with Impact strength, Izod notched, ASTM of 580 J/m | ASTM D 256 |
Streckgrenze | 23.0 °C | 59 MPa Show Material materials with Streckgrenze of 59 MPa | SABIC - Japan Method |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 95 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 95 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6E-5 - 8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6E-5 - 8E-5 1/K | TMA | -30°C to 30°C | ||
Entflammbarkeit | UL Recognized, 94-5VB Flame Class Rating | 2.5mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.4 - 0.6 % Show Material materials with Schrumpfung of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Amusement Machine,ATM/Ticket Machine,Building Accessory,Building Element,Circuit Protection,Cooking Range,Data Management,Data Transfer,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Food Processor,Heavy Vehicles,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Monitoring and Imaging,Non-LED Lighting,Personal Care,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Photovoltaic Components,Power Manangement,Renal and Blood Handling,Respiratory,Security/Detection,Small Appliance,Surgical Devices,Swimming Pool/Spa,Washing Machine,Wireless Communications,Wiring Devices |