Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Material materials with Dichte of 1.19 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.2 % Show Material materials with Wasserabsorption of 0.2 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 2.7 GPa Show Material materials with Biegemodul of 2.7 GPa | ISO 178 | 2 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.7 GPa Show Material materials with Elastizitätsmodul of 2.7 GPa | ISO 527 | 1 mm/min | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527 | 50 mm/min | ||
Flexural yield strength | 23.0 °C | 90 MPa Show Material materials with Flexural yield strength of 90 MPa | ISO 178 | 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 110 MPa Show Material materials with Hardness, Ball Indentation of 110 MPa | ISO 2039-1 | ||
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Material materials with Hardness, Rockwell R of 122 [-] | ISO 2039-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 10 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO 179/1eA | ||
23.0 °C | 15 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 10 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A | ||
23.0 °C | 15 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 15 kJ/m² | ISO 180/1A | |||
Streckgrenze | 23.0 °C | 60 MPa Show Material materials with Streckgrenze of 60 MPa | ISO 527 | 50 mm/min | ||
Zugfestigkeit | 23.0 °C | 50 MPa Show Material materials with Zugfestigkeit of 50 MPa | ISO 527 | 50 mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-30°C | ISO 179/1eU | ||||
Schlagzähigkeit, Izod ungekerbt | No Break @ 23,-30°C| ISO 180/1U |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 80 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ISO 75/Ae | 1.8 MPa | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Relative temperature index, electrical | 80 °C Show Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 70 °C Show Material materials with Relative temperature index, mechanical impact of 70 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 107 °C Show Material materials with Vicat-Erweichungstemperatur of 107 °C | ISO 306 | Rate B/120 | |||
Wärmeleitfähigkeit | 23.0 °C | 0.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.2 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Entflammbarkeit | UL Recognized, 94-5VB Flame Class Rating | 2mm | UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.7 [-] Show Material materials with Dielektrizitätskonstante of 2.7 [-] | IEC 60250 | at 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 17 kV/mm Show Material materials with Durchschlagfestigkeit of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Material materials with Kriechstromfestigkeit of 2 V | UL 746A |
Verlustfaktor | 23.0 °C | 6E-3 [-] Show Material materials with Verlustfaktor of 6E-3 [-] | IEC 60250 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 16 cm³/10min Show Material materials with Schmelzvolumenflussrate of 16 cm³/10min | ISO 1133 | 260°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.4 - 0.6 % Show Material materials with Schrumpfung of 0.4 - 0.6 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Air Conditioning,Air Filtration,Amusement Machine,Animal Testing,ATM/Ticket Machine,Audio,Auto Aftermarket,Building Accessory,Building Element,Circuit Protection,Coffee Maker/Espresso Machine,Commercial Storage/Cookware,Data Management,Data Transfer,Defense Vehicles,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Fluid Delivery,Food Processor,Food Transportation,Forward Lighting,Freezer,Gas/Electric Oven,Heavy Vehicles,Industrial Material Handling,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Microwave Oven,Modular Panel,Monitoring and Imaging,Non-LED Lighting,Personal Care,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Photo/Video Camera,Photovoltaic Components,Plumbing,Power Manangement,Recreational Vehicle,Refrigerator,Renal and Blood Handling,Respiratory,Security/Detection,Small Appliance,Surgical Devices,Surgical Tray,Vacuum Cleaner,Vending Machine,Washing Machine,Watch/Jewelry,Water Treatment/Filtration,Wearables,Window,Wireless Communications,Wiring Devices,Wire & cable | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 2-4hrs, Melt Temperature: 250-270°C, Nozzle Temperature: 250-270°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 240-260°C, Rear - Zone 1 Temperature: 230-250°C, Hopper Temperature: 60-80°C, Mold Temperature: 70-85°C |