Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 4.58 GPa Show Material materials with Biegemodul of 4.58 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 32 % Show Material materials with Dehnung of 32 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 5.2 GPa Show Material materials with Elastizitätsmodul of 5.2 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 99 MPa Show Material materials with Flexural yield strength of 99 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 55 J/m Show Material materials with Impact strength, Izod notched, ASTM of 55 J/m | ASTM D 256 |
23.0 °C | 69 J/m Show Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 5 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A |
23.0 °C | 5 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 58 MPa Show Material materials with Streckgrenze of 58 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 45 MPa Show Material materials with Zugfestigkeit of 45 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 88 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 88 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4.2E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Vicat-Erweichungstemperatur | 108 °C Show Material materials with Vicat-Erweichungstemperatur of 108 °C | ASTM D 1525 | Rate B/50 | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.9E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.9E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94-5VB Flame Class Rating | 2mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 13 g/10min Show Material materials with Schmelzmassenflussrate of 13 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Schmelzvolumenflussrate | 9 cm³/10min Show Material materials with Schmelzvolumenflussrate of 9 cm³/10min | ISO 1133 | 260°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.25 - 0.35 % Show Material materials with Schrumpfung of 0.25 - 0.35 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management,Data Transfer,Displays,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Lab Ware and Clinical Diagnostics,Personal Computing,Wireless Communications | |
Fillers | Mineral Powder | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 245-275°C, Nozzle Temperature: 245-275°C, Front - Zone 3 Temperature: 245-275°C, Middle - Zone 2 Temperature: 220-265°C, Rear - Zone 1 Temperature: 220-255°C, Mold Temperature: 60-80°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 30-80%, Vent Depth: 0.038-0.076mm |