Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Material materials with Dichte of 1.2 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 2.47 GPa Show Material materials with Biegemodul of 2.47 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 35 % Show Material materials with Dehnung of 35 % | ASTM D 638 | Type I, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.68 GPa Show Material materials with Elastizitätsmodul of 2.68 GPa | ASTM D 638 | 50 mm/min | ||
Elongation at yield | 23.0 °C | 4.3 % Show Material materials with Elongation at yield of 4.3 % | ASTM D 638 | Type I, 50 mm/min | ||
Flexural yield strength | 23.0 °C | 95 MPa Show Material materials with Flexural yield strength of 95 MPa | ISO 178 | 2 mm/min | ||
Impact strength, Izod notched, ASTM | -30.0 °C | 109 J/m Show Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D 256 | ||
23.0 °C | 664 J/m Show Material materials with Impact strength, Izod notched, ASTM of 664 J/m | ASTM D 256 | |||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 14 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 14 kJ/m² | ISO 179/1eA | ||
23.0 °C | 45 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 45 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 12 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 12 kJ/m² | ISO 180/1A | ||
23.0 °C | 14 - 20 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 14 - 20 kJ/m² | ISO 180/1A | |||
Streckgrenze | 23.0 °C | 64 MPa Show Material materials with Streckgrenze of 64 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Zugfestigkeit | 23.0 °C | 49 MPa Show Material materials with Zugfestigkeit of 49 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-30°C | ISO 179/1eU | ||||
Schlagzähigkeit, Izod ungekerbt | No Break @ 23,-30°C| ISO 180/1U |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 100 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Relative temperature index, electrical | 90 °C Show Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |
Relative temperature index, mechanical impact | 90 °C Show Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |
Relative temperature index, mechanical strength | 90 °C Show Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |
Vicat-Erweichungstemperatur | 118 °C Show Material materials with Vicat-Erweichungstemperatur of 118 °C | ISO 306 | Rate B/120 | |
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating | 1.5mm | UL 94 |
Elektrisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Material materials with Schmelzvolumenflussrate of 8 cm³/10min | ISO 1133 | 260°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.4 - 0.6 % Show Material materials with Schrumpfung of 0.4 - 0.6 % | SABIC method |
Schrumpfung, diagonal | 23.0 °C | 0.4 - 0.6 % Show Material materials with Schrumpfung, diagonal of 0.4 - 0.6 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Building Element,Building/Construction Sheet,City,Electronic Components,Exterior Rail Components,Non-LED Lighting,Wiring Devices | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 3-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-280°C, Nozzle Temperature: 250-280°C, Front - Zone 3 Temperature: 250-280°C, Middle - Zone 2 Temperature: 245-275°C, Rear - Zone 1 Temperature: 240-270°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-80°C, Drying Temperature: 80-85°C, Drying Time: 2-4hrs, Melt Temperature: 230-270°C, Barrel - Zone 1 Temperature: 235-260°C, Barrel - Zone 2 Temperature: 240-265°C, Barrel - Zone 3 Temperature: 245-270°C, Barrel - Zone 4 Temperature: 245-270°C, Hopper Temperature: 60-80°C, Adapter Temperature: 245-270°C, Die Temperature: 235-260°C |