Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.49 g/cm³ Show Material materials with Dichte of 1.49 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 103 MPa Show Material materials with Biegefestigkeit of 103 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 4.13 GPa Show Material materials with Biegemodul of 4.13 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 389 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 389 J/m | ASTM D 4812 |
Zugfestigkeit | 23.0 °C | 57 MPa Show Material materials with Zugfestigkeit of 57 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 105 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.58E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.58E-5 1/K | ASTM E 831 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.9 [-] Show Material materials with Dielektrizitätskonstante of 2.9 [-] | ASTM D 150 | at 1 MHz |
Durchschlagfestigkeit | 23.0 °C | 16.9 kV/mm Show Material materials with Durchschlagfestigkeit of 16.9 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Verlustfaktor | 23.0 °C | 0.01 [-] Show Material materials with Verlustfaktor of 0.01 [-] | ASTM D 150 | at 1 MHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 1.5 - 1.6 % Show Material materials with Schrumpfung of 1.5 - 1.6 % | SABIC method | 3.2-4.6 mm |
Schrumpfung, diagonal | 23.0 °C | 1.4 - 1.5 % Show Material materials with Schrumpfung, diagonal of 1.4 - 1.5 % | SABIC method | 3.2-4.6 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Aftermarket,Data Management,Forward Lighting,Non-LED Lighting,Rear/Signal Lighting,Recreational Vehicle,Wheel Cover | |
Fillers | Mineral Powder | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |