Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.03 g/cm³ Show Material materials with Dichte of 1.03 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.9 GPa Show Material materials with Biegemodul of 1.9 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 108 % Show Material materials with Dehnung of 108 % | ASTM D 638 | Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 1.68 GPa Show Material materials with Elastizitätsmodul of 1.68 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 3.5 % Show Material materials with Elongation at yield of 3.5 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 57 MPa Show Material materials with Flexural yield strength of 57 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | -30.0 °C | 320 J/m Show Material materials with Impact strength, Izod notched, ASTM of 320 J/m | ASTM D 256 |
23.0 °C | 464 J/m Show Material materials with Impact strength, Izod notched, ASTM of 464 J/m | ASTM D 256 | |
Streckgrenze | 23.0 °C | 35 MPa Show Material materials with Streckgrenze of 35 MPa | ASTM D 638 | Type I, 5 mm/min |
Zugfestigkeit | 23.0 °C | 28 MPa Show Material materials with Zugfestigkeit of 28 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 77 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 77 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.01E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.01E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Schmelzpunkt | 210 - 225 °C Show Material materials with Schmelzpunkt of 210 - 225 °C | ||||
Vicat-Erweichungstemperatur | 106 °C Show Material materials with Vicat-Erweichungstemperatur of 106 °C | ASTM D 1525 | Rate B/50 | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.17E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.17E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating | 1.52mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt viscosity | 23.0 °C | 1520 Pa·s Show Material materials with Melt viscosity of 1520 Pa·s | ASTM D 3825 | 240°C, 100 sec⁻¹ |
Schmelzvolumenflussrate | 4 cm³/10min Show Material materials with Schmelzvolumenflussrate of 4 cm³/10min | ISO 1133 | 220°C/10.0 kg | |
Schrumpfung | 23.0 °C | 0.7 - 0.9 % Show Material materials with Schrumpfung of 0.7 - 0.9 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Electronic Components,Power Boat | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 5-4hrs, Drying Time (Cumulative): 24hrs, Maximum Moisture Content: 0.02-0.04%, Minimum Moisture Content: 0.04%, Barrel - Zone 1 Temperature: 190-220°C, Barrel - Zone 2 Temperature: 190-220°C, Barrel - Zone 3 Temperature: 190-220°C, Barrel - Zone 4 Temperature: 190-220°C, Adapter - Zone 5 Temperature: 195-220°C, Head - Zone 6 - Top Temperature: 195-220°C, Head - Zone 7 - Bottom Temperature: 195-220°C, Screw Speed: 20-60rpm, Extruder Feed Zone Temperature: 60-80°C, Mold Temperature: 40-90°C, Die Temperature: 195-220°C, Drying Temperature: 90-95°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0%, Melt Temperature: 210-240°C, Barrel - Zone 1 Temperature: 195-210°C, Barrel - Zone 2 Temperature: 200-220°C, Barrel - Zone 3 Temperature: 205-230°C, Barrel - Zone 4 Temperature: 210-235°C, Adapter Temperature: 200-225°C, Die Temperature: 210-240°C |