Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Material materials with Dichte of 1.2 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.3 GPa Show Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 120 % Show Material materials with Dehnung of 120 % | ISO 527 | 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.35 GPa Show Material materials with Elastizitätsmodul of 2.35 GPa | ISO 527 | 1 mm/min |
Elongation at yield | 23.0 °C | 6 % Show Material materials with Elongation at yield of 6 % | ISO 527 | 50 mm/min |
Flexural yield strength | 23.0 °C | 90 MPa Show Material materials with Flexural yield strength of 90 MPa | ISO 178 | 2 mm/min |
Streckgrenze | 23.0 °C | 63 MPa Show Material materials with Streckgrenze of 63 MPa | ISO 527 | 50 mm/min |
Zugfestigkeit | 23.0 °C | 70 MPa Show Material materials with Zugfestigkeit of 70 MPa | ISO 527 | 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 135 °C Show Material materials with Vicat-Erweichungstemperatur of 135 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 10 cm³/10min Show Material materials with Schmelzvolumenflussrate of 10 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Window | |
Processing methods | Drying Temperature: 105°C, Drying Time: 2-3hrs, Melt Temperature: 220-250°C, Barrel - Zone 1 Temperature: 240-280°C, Barrel - Zone 2 Temperature: 240-280°C, Barrel - Zone 3 Temperature: 220-240°C, Barrel - Zone 4 Temperature: 220-240°C, Hopper Temperature: 60-80°C, Adapter Temperature: 220-240°C, Die Temperature: 245-290°C |