Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.16 g/cm³ Show Material materials with Dichte of 1.16 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.25 % Show Material materials with Wasserabsorption of 0.25 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.7 GPa Show Material materials with Biegemodul of 2.7 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 49 % Show Material materials with Dehnung of 49 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.68 GPa Show Material materials with Elastizitätsmodul of 2.68 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 4.2 % Show Material materials with Elongation at yield of 4.2 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 78 MPa Show Material materials with Flexural yield strength of 78 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 50 J/m Show Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 |
23.0 °C | 170 J/m Show Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 17 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 17 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 5 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A |
23.0 °C | 17 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 17 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 62 MPa Show Material materials with Streckgrenze of 62 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 48 MPa Show Material materials with Zugfestigkeit of 48 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 89 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 89 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.2E-5 1/K | ASTM E 831 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 105 °C Show Material materials with Vicat-Erweichungstemperatur of 105 °C | ASTM D 1525 | Rate B/50 | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.2E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.2E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 8.3 g/10min Show Material materials with Schmelzmassenflussrate of 8.3 g/10min | ASTM D 1238 | 220°C/10 kg | |
Schmelzvolumenflussrate | 7 cm³/10min Show Material materials with Schmelzvolumenflussrate of 7 cm³/10min | ISO 1133 | 220°C/10.0 kg | |
Schrumpfung | 23.0 °C | 0.5 - 0.7 % Show Material materials with Schrumpfung of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Doors Hardware/Trim,Recreational Vehicle,Seat | |
Processing methods | Drying Temperature: 95-105°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 260-275°C, Nozzle Temperature: 245-265°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 55-70°C, Back Pressure: 0.3-1MPa, Screw Speed: 30-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.038-0.076mm |