Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Material materials with Dichte of 1.04 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.3 GPa Show Material materials with Biegemodul of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 55 % Show Material materials with Dehnung of 55 % | ASTM D 638 | Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.41 GPa Show Material materials with Elastizitätsmodul of 2.41 GPa | ASTM D 638 | 5 mm/min |
Flexural yield strength | 23.0 °C | 75 MPa Show Material materials with Flexural yield strength of 75 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 400 J/m Show Material materials with Impact strength, Izod notched, ASTM of 400 J/m | ASTM D 256 |
Streckgrenze | 23.0 °C | 41 MPa Show Material materials with Streckgrenze of 41 MPa | ASTM D 638 | Type I, 5 mm/min |
Zugfestigkeit | 23.0 °C | 35 MPa Show Material materials with Zugfestigkeit of 35 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Vicat-Erweichungstemperatur | 113 °C Show Material materials with Vicat-Erweichungstemperatur of 113 °C | ASTM D 1525 | Rate B/50 | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.2E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.2E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 2.5 g/10min Show Material materials with Schmelzmassenflussrate of 2.5 g/10min | ASTM D 1238 | 220°C/10 kg | |
Schrumpfung | 23.0 °C | 0.45 - 0.65 % Show Material materials with Schrumpfung of 0.45 - 0.65 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet,Enclosures,Fixture Bath/Shower,Fluid Delivery,Laundry Dryer,Refrigerator,Semiconductor,Washing Machine | |
Processing methods | Drying Temperature: 90-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 230-275°C, Nozzle Temperature: 230-275°C, Front - Zone 3 Temperature: 230-255°C, Middle - Zone 2 Temperature: 210-225°C, Rear - Zone 1 Temperature: 195-210°C, Mold Temperature: 50-80°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm, Drying Temperature: 80-95°C, Drying Time: 4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 215-260°C, Barrel - Zone 1 Temperature: 170-200°C, Barrel - Zone 2 Temperature: 180-220°C, Barrel - Zone 3 Temperature: 190-225°C, Barrel - Zone 4 Temperature: 200-240°C, Adapter Temperature: 205-250°C, Die Temperature: 205-250°C, Roll Stack Temp - Top: 90-95°C, Roll Stack Temp - Middle: 95-105°C, Roll Stack Temp - Bottom: 100-105°C |