Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 80 % Show Material materials with Dehnung of 80 % | ASTM D638 |
Härte, Shore D | 23.0 °C | 43 [-] Show Material materials with Härte, Shore D of 43 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 490 J/m Show Material materials with Impact strength, Izod notched, ASTM of 490 J/m | ASTM D 256 |
Streckgrenze | 23.0 °C | 9 MPa Show Material materials with Streckgrenze of 9 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 10.5 MPa Show Material materials with Zugfestigkeit of 10.5 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 89 °C Show Material materials with Vicat-Erweichungstemperatur of 89 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 7 g/10min Show Material materials with Schmelzmassenflussrate of 7 g/10min | ASTM D1238 | 190°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Caps & closures,Masterbatch |