Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.31 g/cm³ Show Material materials with Dichte of 1.31 g/cm³ | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.08 % Show Material materials with Wasserabsorption of 0.08 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.15 GPa Show Material materials with Biegemodul of 2.15 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 300 % Show Material materials with Dehnung of 300 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.53 GPa Show Material materials with Elastizitätsmodul of 2.53 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 3.6 % Show Material materials with Elongation at yield of 3.6 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 77 MPa Show Material materials with Flexural yield strength of 77 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 50 J/m Show Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 |
23.0 °C | 55 J/m Show Material materials with Impact strength, Izod notched, ASTM of 55 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 5 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A |
23.0 °C | 5 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 56 MPa Show Material materials with Streckgrenze of 56 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 30 MPa Show Material materials with Zugfestigkeit of 30 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 49 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 49 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.7E-5 1/K | ASTM E 831 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 170 °C Show Material materials with Vicat-Erweichungstemperatur of 170 °C | ASTM D 1525 | Rate B/50 | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 8E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt viscosity | 23.0 °C | 400 Pa·s Show Material materials with Melt viscosity of 400 Pa·s | SABIC method |
Schmelzmassenflussrate | 21 g/10min Show Material materials with Schmelzmassenflussrate of 21 g/10min | ASTM D 1238 | 250°C/2.16 kg | |
Schmelzvolumenflussrate | 19 cm³/10min Show Material materials with Schmelzvolumenflussrate of 19 cm³/10min | ISO 1133 | 250°C/2.16 kg | |
Schrumpfung | 23.0 °C | 1.8 - 2.2 % Show Material materials with Schrumpfung of 1.8 - 2.2 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 1.8 - 2.2 % Show Material materials with Schrumpfung, diagonal of 1.8 - 2.2 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device,Renal and Blood Handling,Surgical Devices | |
Processing methods | Drying Temperature: 110-120°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0%, Melt Temperature: 245-260°C, Barrel - Zone 1 Temperature: 200-230°C, Barrel - Zone 2 Temperature: 240-255°C, Barrel - Zone 3 Temperature: 240-275°C, Barrel - Zone 4 Temperature: 240-275°C, Adapter Temperature: 240-275°C, Die Temperature: 240-275°C |