Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.08 g/cm³ Show Material materials with Dichte of 1.08 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 3.52 GPa Show Material materials with Biegemodul of 3.52 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.9 % Show Material materials with Dehnung of 1.9 % | ASTM D 638 | Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 4.08 GPa Show Material materials with Elastizitätsmodul of 4.08 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 1.5 % Show Material materials with Elongation at yield of 1.5 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 36 MPa Show Material materials with Flexural yield strength of 36 MPa | ISO 178 | 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Material materials with Hardness, Rockwell R of 122 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | -30.0 °C | 12 J/m Show Material materials with Impact strength, Izod notched, ASTM of 12 J/m | ASTM D 256 |
23.0 °C | 23 J/m Show Material materials with Impact strength, Izod notched, ASTM of 23 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 1 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 1 kJ/m² | ISO 179/2C |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 1 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 1 kJ/m² | ISO 180/1A |
23.0 °C | 1 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 1 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 48 MPa Show Material materials with Streckgrenze of 48 MPa | ASTM D 638 | Type I, 5 mm/min |
Zugfestigkeit | 23.0 °C | 60 MPa Show Material materials with Zugfestigkeit of 60 MPa | ASTM D 638 | Type I, 5 mm/min |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 98 g/10min Show Material materials with Schmelzmassenflussrate of 98 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Plastic |