Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.09 g/cm³ Show Material materials with Dichte of 1.09 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 3.62 GPa Show Material materials with Biegemodul of 3.62 GPa | ISO 178 | 2 mm/min |
Flexural yield strength | 23.0 °C | 58 MPa Show Material materials with Flexural yield strength of 58 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 13 J/m Show Material materials with Impact strength, Izod notched, ASTM of 13 J/m | ASTM D 256 |
23.0 °C | 19 J/m Show Material materials with Impact strength, Izod notched, ASTM of 19 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 1 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 1 kJ/m² | ISO 179/2C |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 1 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 1 kJ/m² | ISO 180/1A |
23.0 °C | 3 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 3 kJ/m² | ISO 180/1A | |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 21 g/10min Show Material materials with Schmelzmassenflussrate of 21 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Cladding/Roof |