Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.07 g/cm³ Show Material materials with Dichte of 1.07 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 3.4 GPa Show Material materials with Biegemodul of 3.4 GPa | ISO 178 | 2 mm/min |
Flexural yield strength | 23.0 °C | 38 MPa Show Material materials with Flexural yield strength of 38 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 18 J/m Show Material materials with Impact strength, Izod notched, ASTM of 18 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 1 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 1 kJ/m² | ISO 180/1A |
23.0 °C | 2 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 2 kJ/m² | ISO 180/1A | |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0 g/10min Show Material materials with Schmelzmassenflussrate of 0 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures |