Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Material materials with Dichte of 1.2 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.42 GPa Show Material materials with Biegemodul of 2.42 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 119 % Show Material materials with Dehnung of 119 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.22 GPa Show Material materials with Elastizitätsmodul of 2.22 GPa | ASTM D 638 | 50 mm/min |
Elongation at yield | 23.0 °C | 7 % Show Material materials with Elongation at yield of 7 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 97 MPa Show Material materials with Flexural yield strength of 97 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | -30.0 °C | 44 J/m Show Material materials with Impact strength, Izod notched, ASTM of 44 J/m | ASTM D 256 |
23.0 °C | 581 J/m Show Material materials with Impact strength, Izod notched, ASTM of 581 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2140 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 2140 J/m | ASTM D 4812 |
Streckgrenze | 23.0 °C | 61 MPa Show Material materials with Streckgrenze of 61 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 59 MPa Show Material materials with Zugfestigkeit of 59 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 124 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.8E-5 1/K | ASTM E 831 | -40°C to 95°C |
Vicat-Erweichungstemperatur | 142 °C Show Material materials with Vicat-Erweichungstemperatur of 142 °C | ISO 306 | Rate B/120 | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.6E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.6E-5 1/K | ASTM E 831 | -40°C to 95°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 58 g/10min Show Material materials with Schmelzmassenflussrate of 58 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.6 - 0.9 % Show Material materials with Schrumpfung of 0.6 - 0.9 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 295-315°C, Nozzle Temperature: 290-310°C, Front - Zone 3 Temperature: 295-315°C, Middle - Zone 2 Temperature: 280-305°C, Rear - Zone 1 Temperature: 270-295°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |