Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.96 g/cm³ Show Material materials with Dichte of 0.96 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 23 MPa Show Material materials with Biegefestigkeit of 23 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 0.83 GPa Show Material materials with Biegemodul of 0.83 GPa | ISO 178/1A |
Härte, Shore D | 23.0 °C | 60 [-] Show Material materials with Härte, Shore D of 60 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 24 MPa Show Material materials with Streckgrenze of 24 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 12 MPa Show Material materials with Zugfestigkeit of 12 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 124 °C Show Material materials with Vicat-Erweichungstemperatur of 124 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Caps & closures,Houseware & appliances |