Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527-2 1A | 1mm/min |
Elongation at yield | 23.0 °C | 9 % Show Material materials with Elongation at yield of 9 % | ISO 527-2 1A |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5.6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 5.6 kJ/m² | ISO 179 |
Streckgrenze | 23.0 °C | 63 MPa Show Material materials with Streckgrenze of 63 MPa | ISO 527-2 1A | 50 mm/min |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Material materials with Schmelzvolumenflussrate of 8 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive |